Atomic Layer Deposition of Aluminum Nitride Thin Films from Trimethyl Aluminum (TMA) and Ammonia

Publication Type : Conference Proceedings

Publisher : Cambridge Univ Press

Source : MRS Proceedings, Cambridge Univ Press, p.11-18 (2004)

Campus : Coimbatore

School : School of Engineering

Department : Chemical

Verified : Yes

Year : 2004

Abstract : luminum nitride (AlN) thin films were deposited from trimethyl aluminum (TMA) and Ammonia (NH3) by thermal atomic layer deposition (thermal ALD) and plasma enhanced atomic layer deposition (PEALD) on 200 mm silicon wafers. For both thermal ALD and PEALD, the deposition rate increased significantly with the deposition temperature. The deposition rate did not fully saturate even with 10 seconds of NH3 pulse time. Plasma significantly increased the deposition rate of AlN films. A large number of incubation cycles were needed to deposit AlN films on Si wafers. 100% step coverage was achieved on trenches with aspect ratio of 35:1 at 100 nm feature size by thermal ALD. X-ray diffraction (XRD) data showed that the AlN films deposited from 370 °C to 470 °C were polycrystalline. Glancing angle X-ray reflection (XRR) results showed that the RMS roughness of the films increased as the film thickness increased.

Cite this Research Publication : X. Liu, Dr. Sasangan Ramanathan, Lee, E., and Seidel, T. E., “Atomic Layer Deposition of Aluminum Nitride Thin Films from Trimethyl Aluminum (TMA) and Ammonia”, MRS Proceedings. Cambridge Univ Press, pp. 11-18, 2004.

Admissions Apply Now
OSZAR »